i_1C 17.5[A/m^2] 1C discharge current Ds_neg 3.9e-14[m^2/s] Solid phase Li-diffusivity Negative Ds_pos 1e-13[m^2/s] Solid phase Li-diffusivity Positive rp_neg 12.5e-6[m] Particle radius Negative rp_pos 8e-6[m] Particle radius Positive T 298[K] Temperature epss_pos 1-epsl_pos-0.259 Solid phase vol-fraction Positive epsl_pos 0.444 Electrolyte phase vol-fraction Positive cl_0 2000[mol/m^3] Initial electrolyte salt concentration epss_neg 1-epsl_neg-0.172 Solid phase vol-fraction Negative epsl_neg 0.357 Electrolyte phase vol-fraction Negative csmax_neg 26390[mol/m^3] Max solid phase concentration Negative csmax_pos 22860[mol/m^3] Max solid phase concentration Positive cs0_neg 14870[mol/m^3] Initial Negative State of Charge cs0_pos 3900[mol/m^3] Initial Positive State of Charge k_neg 2e-11[m/s] Reaction rate coefficient Negative k_pos 2e-11[m/s] Reaction rate coefficient Positive L_neg 100e-6[m] Length of negative electrode L_sep 52e-6[m] Length of separator L_pos 183e-6[m] Length of positive electrode i_app a*i_1C Discharge current for parametric study of lumped model R_solution 3.5e-3[ohm*m^2] Solution phase resistance in the cell a 1 Multiplicative factor for the parametric study